A buyer we were quoting this month asked for the 3.1 before he would talk about price. He did not want a sample, and he did not ask to visit a factory. He wanted to see what the sheet looks like when it comes from the mill we actually buy from, because he had been sent certificates before that turned out to belong to a different batch.
That is the right question to ask early. A 3.1 is not a guarantee of quality, and it is not a certificate issued by an independent body. It is a report of measured results for one batch of steel, signed by the mill’s own inspection department. What it covers, and where it stops, decides whether a shipment is accepted on arrival.
It is not a third-party certificate
Most buyers expect a 3.1 to come from a laboratory. It arrives instead on mill paper, with the mill’s heading and one signature at the bottom, and the first reaction is that it has been forged.
Under EN 10204, the 3.1 is an inspection certificate issued by the manufacturer, with the actual test results stated for each item. The person who signs it must be independent of the production department. He works for the mill, but he does not run the line, and he answers for the figures.
That independence is the whole difference between 3.1 and 2.2. A 2.2 is a declaration of compliance: it may state that the goods meet the order and give no measured values at all. A 3.1 has to give the numbers.
A certificate from a genuinely independent body is a 3.2, or a separate inspection report from SGS, BV or TUV commissioned by the buyer. These are two different documents, and one cannot stand in for the other.
So a 3.1 bearing only the mill’s name is normal. A document headed 3.1 that carries an SGS logo but no SGS report number is the one to question.
Three identities have to be on the sheet
A 3.1 that can be used carries three references in the heading: the manufacturer’s name and address, the purchase order or contract number, and the certificate number. Miss any one and the sheet cannot be tied to a particular consignment.
The manufacturer field names the producing mill, not the trading company. That is what allows the certificate to travel with the goods and to hold up at site acceptance, where the engineer reads who made the batch.
Below that is the signature block: the name, position, signature and date of the inspection representative. A stamp without a signature is generally not accepted in Europe.
The heat number is the only hard link
The one field that genuinely connects the paper to the steel is the heat number.

A 3.1 is normally issued per heat, and a single heat can cover several sizes from the same cast and the same heat treatment batch. A certificate listing seven sizes from half inch to six inch is therefore normal, not a way of covering a shortage. The test is not one certificate per size. The test is whether the heat number stamped on the fitting appears on that certificate.
Under B16.9 the heat number is a required mark on the fitting, together with the grade, the size, the wall thickness or schedule, and the manufacturer’s symbol. Under B16.5 the heat number is marked when the order specifies it. On flanges, check the order first: no requirement and no mark is not a defect; a requirement and no mark is a different matter.
The sequence is: heat number on the fitting, same heat number on the certificate, chemical and mechanical results for that heat, then the same number on the packing list and the shipping marks. Four places in agreement closes the batch. Any disagreement, and the case stays open.
The lines worth reading
Four blocks are enough. They are the four that come back as claims after the goods land.
Chemistry: carbon, manganese, phosphorus and sulphur first. Phosphorus and sulphur above the limit are the most common reason for rejection. A105 allows phosphorus to 0.035 and sulphur to 0.040. A234 WPB is wider, at 0.050 and 0.058. A WPB certificate showing sulphur at 0.045 is compliant; the same figure on an A105 is not. One number, two standards, two verdicts.
Mechanics: A105 requires tensile strength of at least 485 MPa, yield of at least 250 MPa, and elongation of at least 22 percent. WPB requires 415 to 585 MPa tensile and 240 MPa yield. Below the minimum is a rejection. Above the maximum is a question, because a WPB heat over 585 MPa is stronger than the specification intends and may be short on toughness.
Heat treatment: normalized, annealed, solution annealed. If the line is there, the treatment was done; if it is absent, it was not. A buyer who specified normalizing and receives a certificate without that line has goods that do not meet the order, however good they look.
Standard and edition: ASTM A105/A105M with the year of the edition, or SA-105 for the ASME adoption. An edition ten years old is worth a question about which version the mill actually worked to.
A105 or SA105, F304 or 304
This is where Chinese certificates are most often challenged, and usually without cause.
ASTM and ASME are two systems. The same material is A105 under ASTM; when ASME adopts it, the designation takes an S and becomes SA-105. Stainless forgings follow the same rule: A182 F304 becomes SA-182 F304. Pressure equipment and piping projects work to ASME, so SA- on the certificate is correct. A- is not wrong, but a project inspector may return it for reissue.
The distinction that does matter is F304 against 304. F304 is a forging grade from A182. 304 is the general stainless grade, from A240 plate or A312 pipe. A forged flange certified as 304, or plate certified as F304, is a mismatch of product form. The two are mixed up in Chinese documentation often enough to be worth checking.
Three things a 3.1 does not prove
This part is rarely explained, and every buyer meets it sooner or later.
First, it does not prove that non-destructive testing was performed. Radiography, ultrasonic, penetrant and magnetic particle each produce their own report. A 3.1 may state that the goods were tested to a standard; it will not show you the film.
Second, it does not prove dimensional compliance. Dimensions are a separate report. Face finish on a flange, bolt hole centre distance, squareness of an elbow: none of these appear on a 3.1.
Third, it does not prove where the raw steel came from. Unless the certificate names the steel mill and its own heat number, the 3.1 covers the finished product only, and the step before it is blank. Tracing to the steelworks requires the raw material certificate as well.
Knowing these three limits lets a buyer ask for the full set at the quotation stage: 3.1, NDT report, dimensional report, raw material certificate. Assembling them before shipment is far quicker than chasing them after arrival.
How the documents are issued
The certificate is issued by the producing mill, with the mill named as manufacturer, our order number on the sheet, and measured results for each heat. We make 3.1 a condition of the purchase order, not a favour requested afterwards.
The heat number is written to match in three places: the mark on the fitting, the packing list and the certificate. An order spanning several heats receives several certificates; they are not combined onto one sheet.
Where a project requires third-party witnessing, the inspection plan is sent before production starts, and the fee and lead time for SGS or BV are quoted separately from the goods.
A 3.1 that arrives after the goods are unloaded is worth very little. Ask for it with the quotation, not with the container.
Once the sheet is in hand, the four points that decide acceptance are set out in how to check a 3.1 certificate.